ua Zoo tshaj Superalloy Inconel625/ UNS N06625/ Alloy625 Chaw tsim tshuaj paus Chaw tsim tshuaj paus thiab tsum |Guojin

Superalloy Inconel625 / UNS N06625 / Alloy625 Chaw tsim tshuaj paus

Lus piav qhia luv luv:

Qib sib npaug:
UNS N06625
DIN W. Nr.2.4856 ib


Product Detail

Khoom cim npe

Cov khoom muaj

Seamless raj, phaj, pas nrig, forgings, fasteners, yeeb nkab fittings

Cov qauv tsim

Khoom

ASTM

Bar

ib 446

Phaj, Sheet thiab Sawb

ib 443b906

Seamless yeeb nkab, raj

ib 444b829

Welded yeeb nkab

Ib 705, B 775

Welded fittings

ib 704b751

Welded connectors

ib 366

Forged billets thiab tuav

ib 472

Forging

ib 564

Tshuaj muaj pes tsawg leeg

%

Ni

Cr

Mo

Fe

C

Mn

Si

P

S

Co

Nb+Ta

Al

Ti

Min

58.0 ua

20.0 Nws

8.0 ib

3.15

Max

23.0 Nws

10.0

5.0

0.10

0.50 ib

0.50 ib

0.015 ib

0.015 ib

1.00 Nws

4.15

0.40 Nws

0.40 Nws

Lub cev muaj zog

Qhov ntom

8.36 ibg/cm3

Melting

1330-1375 ℃

Inconel 625 nta

1. Zoo heev corrosion kuj rau ntau yam corrosive media hauv oxidizing thiab txo qhov chaw
2. Zoo heev rau pitting corrosion thiab crevice corrosion, thiab yuav tsis tsim chloride ion kev nyuaj siab corrosion cracking
3. Zoo heev corrosion kuj rau inorganic acids, xws li nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid thiab sib xyaw acids ntawm sulfuric acid thiab hydrochloric acid, thiab lwm yam.
4. Zoo heev tiv thaiv corrosion ntawm ntau yam inorganic acid tov tov
5. Thaum qhov kub nce mus txog 40 ℃, nws tuaj yeem pom zoo corrosion kuj nyob rau hauv ntau qhov ntau ntawm hydrochloric acid tov.
6. Kev ua haujlwm zoo thiab weldability, tsis muaj kev sib tsoo tom qab vuam
7. Kev tsim cov ntawv pov thawj ntawm cov hlab ntsha siab nrog cov phab ntsa kub ntawm -196 ~ 450 ℃
8. Muaj ntawv pov thawj los ntawm American Society of Corrosion Engineers NACE tus qauv (MR-01-75) kom ua tau raws li tus txheej txheem siab tshaj plaws VII rau kev siv hauv cov roj qaub.

Inconel625 Daim Ntawv Thov Cheeb Tsam

Lub softened thiab annealed uas tsis muaj carbon alloy 625 yog dav siv nyob rau hauv cov txheej txheem tshuaj, thiab nws zoo corrosion kuj thiab siab zog pab kom nws yuav siv tau raws li ib tug nyias txheej txheej.Alloy 625 tuaj yeem siv rau hauv cov ntawv thov raug dej hiav txwv thiab raug rau cov neeg kho tshuab siab.Tej thaj chaw thov:
1. Cov txheej txheem ntawm cov txheej txheem tshuaj lom neeg muaj cov tshuaj chlorides, tshwj xeeb tshaj yog siv cov kua qaub chloride catalysts.
2. Digesters thiab bleaching tanks rau kev lag luam pulp thiab ntawv
3. Absorption ntauwd, reheater, flue gas inlet baffle, kiv cua (humid), agitator, deflector thiab flue hauv flue gas desulfurization system
4. Rau kev tsim cov khoom siv thiab cov khoom siv rau hauv qhov chaw qaub roj
5. Acetic acid thiab acetic anhydride cov tshuaj tiv thaiv generator
6. Sulfuric acid condenser